Abstract: With the process measures including using low titanium hot metal, alloys and slagging materials, eccentric bottom tapping and alloying in tapping in EAF steelmaking, using Si-Al compound deoxidation and CaO-MgO-SiO2 -Al2O3 slag series with basicity 3 ~5 in LF refining,30 Pa VD treatment and shielding casting,the analysis results of Φ150 mm forged bar are oxygen content in GCrl5 bearing steel being 4.5 X 10-6 ~9 x 10-6 ,Ti content 0.0010% ~0.0015% with minor 5 μm TiN inclusions to meet the quality requirement for super grade quality low titanium bearing steel.
邬中华. 太钢60 t EAF-LF-VD-2.5 t铸锭流程冶炼低钛轴承GGrl5钢的实践[J]. 特殊钢, 2019, 40(1): 57-59.
Wu Zhonghua. Practice of Low Titanium Bearing Steel GCrl5 Steelmaking by 60 t EAF-LF-VD-2.5 t Ingot Flowsheet at Taigang[J]. Special Steel, 2019, 40(1): 57-59.
0 / / 推荐
导出引用管理器 EndNote|Ris|BibTeX
链接本文: https://www.specialsteeljournal.com/CN/
https://www.specialsteeljournal.com/CN/Y2019/V40/I1/57