70CaF2-30Al2O3渣系电渣重熔Cr13Mn4Mo不锈钢中夹杂物的演变

张钊1,2,刘昱1,2,李光强1,2,王强1,2,袁成1,2,王力1,2   

  1. 1. 武汉科技大学耐火材料与冶金省部共建国家重点实验室;
    2. 钢铁冶金及资源利用省部共建教育部重点实验室,武汉430081
  • 收稿日期:2017-06-25 出版日期:2017-12-01 发布日期:2022-07-06
  • 作者简介:张钊(1993-),男,硕士研究生,2015年武汉科技大学(本科)毕业,钢水精炼的研究。
  • 基金资助:
    大截面超洁净双性能汽轮机转子真空电渣重熔制备的科学基础(编号:U1508214)

Evolution of Inclusions in Stainless Steel Cr13Mn4Mo Electroslag-Remelted by 70CaF2-30Al2O3 Slag Series

Zhang Zhao1,2, Liu Yu1,2, Li Guangqiang1,2, Wang Qiang1,2, Yuan Cheng1,2, Wang Li1,2   

  1. 1. State Key Laboratory of Refractories and Metallurgy,
    2. Key Laboratory of Ferrous Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081
  • Received:2017-06-25 Published:2017-12-01 Online:2022-07-06

摘要: 采用70CaF2-30Al2O3渣系对Cr13Mn4Mo钢进行电渣重熔试验。利用SEM/EDS、氧氮分析仪和碳硫分析仪分析和检测了Ф55mm电极及Ф120mm(36kg)电渣锭中全氧含量、硫含量及夹杂物的数量、尺寸和形貌,钢中MnS夹杂的析出过程进行了热力学分析。结果表明,电渣重熔后钢中全氧含量由0.0121%降低至0.0044%,硫含量由0.010%降低至0.002%,和电极相比,电渣锭中夹杂物数密度由855个/mm2降低至257个/mm2,钢中夹杂物的尺寸明显减小,为1μm左右Al2O3夹杂,以及以Al2O3为核心,外层附着MnS的复合夹杂。热力学计算表明,在实验条件下没有单个的MnS生成,这与SEM/EDS分析结果吻合。

关键词: 电渣重熔, Cr13Mn4Mo不锈钢, 夹杂物演变, MnS, 二次枝晶臂

Abstract: The electroslag-remelting (ESR) test on steel Cr13Mn4Mo by 70CaF2-30Al2O3 slag series has been carried out. The total oxygen content, sulfur content and amount, size and morphology of inclusions in Ф55mm electrode and Ф120mm (36kg) ESR ingot are analyzed and measured by SEM/EDS, oxygen-nitrogen determinator and carbon-sulfur analyzer, and the thermodynamic analysis on MnS inclusions precipitation process in steel is carried out. Results show that by ESR the total oxygen content in steel decreases from 0.0121% to 0.0044%, sulfur content in steel decreases from 0.010% to 0.002% , as compared with electrode the number per mm2 of inclusions in ESR ingot decreases from 855 to 257 and the size of inclusions in ESR ingot decreases obviously which are about 1μm Al2O3 and compound inclusions with Al2O3 core surrounded by MnS at outside. Thermodynamic calculated results show that in test conditions there is no single MnS formation that agrees with SEM/EDS analysis results.