ISSN:1003-8620

CN:42-1243/TF

主管:中信泰富特钢集团股份有限公司

主办:大冶特殊钢有限公司

特殊钢 ›› 2014, Vol. 35 ›› Issue (6): 5-8.

• 试验研究 • 上一篇    下一篇

石油套管用钢37Mn5 Φ210 mm连铸圆坯凝固过程的数学模拟和工艺优化

朱新华1,2,朱立光2,孙向东2,孟娜2   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2河北联合大学冶金与能源学院,唐山063009
  • 收稿日期:2014-08-20 出版日期:2014-12-01 发布日期:2022-08-19
  • 通讯作者: 朱立光
  • 作者简介:朱新华(1977-),女,博士生(北京科技大学),副教授,2001年河北理工大学(本科)毕业,连铸工艺研究。
  • 基金资助:
    国家自然科学基金项目资助(51074063)

Mathematic Simulation on Solidification Process of Φ210 mm Cast Round Bloom of Steel 37Mn5 for Petroleum Sleeve Tube and Process Optimization

Zhu Xinhua1,2 , Zhu Liguang2 , Sun Xiangdong2 , Meng Na2   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083 ;
    2 School of Metallurgy and Energy Engineering, Hebei United University, Tangshan 063009
  • Received:2014-08-20 Published:2014-12-01 Online:2022-08-19

摘要: 在分析37Mn5钢(/%:0.34~0.39C,0.20~0.35Si,1.25~1.50Mn)凝固特性的基础上通过用ANSYS软件建立连铸圆坯凝固热-力耦合数学模型,对Φ210 mm连铸圆坯凝固过程进行模拟,分析了40 t中间包,拉速1.4 m/min,浇铸温度1531℃时,二冷水比水量0.58~0.78 L/kg和各段配置对铸坯表面温度、坯壳厚度、液芯长度和表面应力的影响。模拟结果表明,比水量每增加0.1 L/kg,铸坯表面约下降18℃,试验比水量变化对出口坯壳厚度、液芯长度和表面应力影响不显著,但原工艺配水量0.68 L/kg下二冷0段和1段之间空冷部位出现高达185℃急速回温,最大应力达6.41×107Pa,通过保持配水量0.68 L/kg不变,调整各段配水量使0~1段间回温降至123℃,最高应力降至4.53×107Pa,铸坯裂纹基本消失,表面质量显著改善。

关键词: 石油套管用钢37Mn5, Φ210 mm坯连铸, 二冷制度, 数学模拟, 表面质量

Abstract: Based on analysis on solidification characteristics of steel 37Mn5 (/% : 0. 34 ~0. 39C, 0. 20 ~ 0. 35Si, 1. 25 ~ 1. 50Mn) during casting, a thermal-mechanical coupled mathematical model is established by using software ANSYS to simulate the solidification process of Φ210 mm casting round bloom and analyze with 40 t tundish, casting rate 1. 4 m/min and casting temperature 1 531 °C the effect of secondary cooling water ratio 0.58 ~ 0. 78 L/kg and distribution of water rate at each section on casting bloom surface temperature, shell thickness, length of liquid core and surface stress. The simulation results show that with increasing secondary cooling water ratio by per 0. 1 L/kg the bloom surface temperature decreases by about 18 ℃,while the effect of testing cooling water ratio on shell thickness at outlet of mold, length of liquid core and surface stress is not obvious. But with cooling water ratio 0. 68 L/kg the rapid re-raise temperature of bloom occurs by 185 °C in air cooling region between 0 and 1 section for original process and the max stress is up to 6. 41 X 107 Pa. With maintaining the same cooling water ratio 0. 68 L/kg, to control the re-raise temperature range decreases to 123 ℃ and the highest stress decreases to 4. 53 x 107 Pa, as a result the bloom cracks basically dismiss and the surface quality of bloom improves markedly.