[1]Viswanathan R,Bakker W T,超超临界火电厂锅炉用材的开发 [J] 世界钢铁,2007,7(2):3446.
[2]Lu Yansun. Development of China Electricity Industry and Power Plant Equipment Materials [ C ] 〃 2009 Symposium on Advanced Power Plant Heat Resistant Steels and Alloys,2009.
[3]唐利萍.超超临界锅炉用钢的发展[J].应用能源技术,2007 (10):20-21.
[4]Chen Qiurong, Helmrich A, Weissinger G. Experiences With Boiler Materials for 600 °C Power Plants and New Development Activities for Highest Steam Parameters [C] // 2009 Symposium on Advanced Power Plant Heat Resistant Steels and Alloys ,2009.
[5]艾国安,谷力功,曹 俊.高压锅炉管生产现状[J].天津冶金, 2006(1) :18-22.
[6]钟倩霞,张艳红,严圣祥.加快开发和生产火电锅炉耐热钢管 [N].中国冶金报,2011-11-22(004).
[7]杨 富.我国超超临界机组金属与焊接的现状与展望[C],超超 临界机组技术交流年会,天津,2013,1,11.
[8]王起江,邹凤鸣,赵群义.宝钢T23高压锅炉管的研制[J].宝钢 技术,2006(1):59-62.
[9]Nippon Steel & Sumitomo Metal: Detailed Information by Product [OL].新日铁住金产品手册,http: //www. nssmc. com/product/ catalog_download/pdf/P008en, pdf
[10]何晓梅,罗昌福,刘漫博.超超临界火电机组的选材及国产化进程[JL材料热处理技术,2012,41(22):116-124.
[11]杨 岩,程世长,杨 钢.铜含量对Super304H钢持久性能的影响[J].机械工程材料,2002,26(10):23-25.
[12]王剑志,罗仕清,黄晓斌.超(超)临界锅炉用S叩er304H钢管研究试制[J]-钢铁,20。6,41(1) :4346.
[13]彭芳芳,朱国良,宋建新.超超临界机组用SUPER304H钢管国产化关键制造工艺的分析□].动力工程,2008,28(5)=803- 806.
[14]王剑志,罗仕清,黄晓斌.超(超)临界锅炉用SUPER304H钢管试制研究[J].特钢技术,2005(1):1-6.
[15 ] Masuyam A F. Lessons on Material Issues from Eddy Stone USC Power Plant [ C ] 〃2009 Symposium on Advanced Power Plant Heat Resistant Steels and Alloys ,2009.
[16]于鸿盅,董建新,谢锡善.新型奥氏体耐热钢HR3C的研究进展 [J]世界钢铁,2010,10(2):4249.
[17]王敬忠,程世长,刘正东.HR3C钢高温拉伸塑性偏低的影响因素研究[C] 〃先进电站用耐热钢与合金研讨会.上海:2009.
[18]Danielsen H K, Hald J. Tantalum-Containing Z-Phase in 12% Cr Martensitic Steels[J]. Scripta Materialia,2009,60 (9):811-813.
[19]Danielsen H K, Hald J. A Thermodynamic Model of the Z PhaseCr(V,Nb) N [J].Calphad December 2007,31 (4) :505-514.
[20]Cipolla L,Danielsen H,Venditti D,et al. Conversion of MX Nitrides to Z-Phase in a Martensitic 12% Cr Sttel[J]. Acta Materialia,2010 (58):669-679.
[21] Danielsen H K,Hald J. On the Nucleation and Dissolution Process of Z-Phase Cr( V,Nb)N in Martensitic 12% Cr Steels[J]. Materials Science and Engineering: A,2009,505(1):169-177.
[22] Nippon Steel & Sumitomo Metal: Detailed Information by Product [OL]. ,新日铁住金产品介绍,http: //www. tubular, nssmc.com/ product-services/specialty-tube/tube-application/fossil-fuel-power.
[23]JFE:Detailed Information by Product[ OL]. JFE 产品介绍,http: // www. jfe-steel. co. jp/ch/products/
[24]慧 子.JFE钢铁公司能源工业用钢[N].世界金属导报,2013- 4-9(14)
[25]JFE:Detailed Information by Product [OL]. JFE 技术报告,http: // www. jfe-steel. co. jp/en/products/list. html#Pipes-&-Tubes
[26]Sandvik: Detailed Information by Product [OL]. Sandvik 产品手 册,http: //www. smt. sandvik. com/Global/Downloads/Products_ downloads/tubular-products/S-1211 l-ENG-050822. pdf
[27]顾建忠.国外双层金属复合钢管的用途及生产方法[J]-±海 金属,2000,22(4):16-24.
[28]孙育禄,白真板,张国超,油气田防腐用双金属复合管研究现状 [J]. TOTAL CORROSION CONTROL,2011,25(5):1(M6.
[29]Kimb Y U,Kwunb S I,Shima J H,et al. The Effect of Cooling Conditions after Solution Treatment on the Creep Rupture Strength of Sanicro25 : A Materials Science and Technology Research Division [OB/OL]. Korea Institute of Science and Technology (KIST). Seoul,2009:136.
[30]Shim Jae-Hyeok, Kozeschnik Ernst, Jung Woo-Sang, et al. Numerical Simulation of Long-Term Precipitate Evolution in Austenitic Heat-Resistant Steels[J]. Calphad,2010,34(1) :105-112.
[31] Sandvik:Detailed Information by Product [OL]. Sandvik 产品手册,http:〃www. smt. sandvik. com/en/materials-center/material- datasheets/tube-and-pipe-searnless/sanicro--25/
|