100 t EAF-LF-VD-CC流程冶炼非调质钢49MnVS3的工艺实践

代刚,朱志红   

  1. 江苏苏钢集团苏信特钢有限公司电炉厂,苏州215151
  • 收稿日期:2015-02-07 出版日期:2015-08-01 发布日期:2022-08-25
  • 作者简介:代 刚(1980-),男,炼钢工艺工程师,2004年武汉科技大学毕业,非调质钢的生产工艺研究。

Process Practice of Non-Quenched-Tempered Steel 49MnVS3 Steelmaking by 100 t EAF-LF-VD-CC Flowsheet

Dai Gang ,Zhu Zhihong   

  1. Electric Arc Furnace Works, Suxin Special Steel Co Ltd, Jiangsu Susteel Group, Suzhou 215151
  • Received:2015-02-07 Published:2015-08-01 Online:2022-08-25

摘要: 10炉非调质钢49MnVS3(/%:0.46~0.48C,0.30~0.40Si,0.88~0.92Mn,0.001~0.014P,0.004~0.005S,0.09~0.10V,0.19~0.22Cr)由100 t EBT DC EAF-LF-VD-260 mm×340 mm坯连铸-Φ140~150 mm材轧制流程生产。采用兑入75%铁水,EAF前期脱磷至≤0.015%P,出钢前[C]为0.20%~0.30%,精炼时加150~200kg碳化硅,控制LF精炼渣碱度2.80~2.95,(CaO)/(Al2O3)=1.2~1.6,VD后喂1.5 m/t钙铁线,软吹时间≥15min等工艺措施,49MnVS3钢中[N]、[H]和[O]分别为130×10-6~220×10-6,1.2×10-6~1.5×10-6和5×10-6~11×10-6,成品材晶粒度≥5级,非金属夹杂物和低倍组织均≤1.5级,组织(带状≤1级)和力学性能(R803~883 MPa,Rel 517~590 MPa, A 16%~21%,Aku 39~99 J)均满足标准要求。

关键词: 100 t DC EAF-LF-VD-CC流程, 非调质钢49MnVS3, 工艺实践

Abstract: 10 heats of non-quenched-tempered steel 49MnVS3 (/% : 0.46 ~ 0.48C, 0,30 ~ 0.40Si, 0.88〜0.92Mn, 0.001~0. 014P, 0.004 ~ 0.005S, 0.09~ 0.10V, 0.19 ~ 0.22Cr) are produced by 100 t EBT DC EAF-LF- VD-260 mm x 340 mm bloom casting-Φ140 〜150 mm round bar rolling process flowsheet. With using the process measures including charging 75% hot metal, in EAF earlier period dephosphorizing to ≤0.015%P, before tapping controlling 0.20% ~0. 30% [C] , in refining adding 150 ~200 kg silicon carbide, controlling LF refining slag basicity 2. 80 ~2. 95 and ( CaO)/( Al2O3) = 1.2 ~ 1. 6, after VD feeding 1. 5 m/t calcium-iron wire and soft argon blowing for ≥15 min, the [N] , [H] and [O] of steel 49MnVS3 are respectively 130 x 10-6 - 220 x 10-6, 1.2 x 10-6 - 1.5 x 10-6 and 5 x 10-6 ~ 11 x 10-6 , finished products grain size is N5 rating, nonmetallic inclusions and macrostructure are all ≤ 1. 5 rating, the structure (banded orientation ≤1 rating) and the mechanical properties (R803 ~883 MPa, Rel 517 〜590 MPa, A 16% ~21%, Aku39~59J) all meet the requirement of standard.