国内1215系低碳高硫易切削钢的工艺流程和内部质量控制

林腾昌, 朱荣,王成杰, 李文双, 马国宏   

  1. 北京科技大学冶金与生态工程学院,北京100083
  • 收稿日期:2013-02-20 出版日期:2013-08-01 发布日期:2022-09-11
  • 作者简介:林腾昌(1986-),男,博士研究生.2008年太原理工大学学业,特殊钢工艺开发及质量控制研究:

Process Flow Sheet and Internal Quality Control of Domestic 1215 Low Carbon High Sulphur Free-Cutting Steel

Lin Tengchang, Zhu Rong, Wang Chengjie, Li Wenshuang , Ma Guohong   

  1. School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083
  • Received:2013-02-20 Published:2013-08-01 Online:2022-09-11

摘要: 对国内100 t EAF-LF-CC和80 t、100 t、160 t转炉-LF-CC四条生产线生产的1215系低碳高硫易切削钢(/%:0.05~0.10C、≤0.013Si、1.06~1.33Mn、0.051~0.061P、0.24~0.36S、0.012 0~0.0140[O]、≤0.005Al)进行实物分析。结果表明,国内1215低碳高硫钢成分控制特点为通过适当提高Mn含量控制钢中的Mn/S (3.7~3.9),个别流程通过降低S含量可使Mn/S达4.4;160 t转炉流程在夹杂物控制上优于其余流程(Mn/S=3.8, MnS夹杂面积和长宽比波动较小)。.由于连铸坯元素偏析较小和轧后冷却速度控制得当,80 t转炉流程和160 t转炉流程生产的钢中无明显的带状组织,而100 t电弧炉流程和100 t转炉流程生产的钢中带状组织级别为3~4。

Abstract: An analysis on the products of 1215 low carbon high Sulphur free-cutting steel (/%: 0. 05 ~ 0. 10C, W 0.013Si, 1.06 ~1.33Mn, 0. 051 -0.061P, 0. 24 ~0. 36S, 0.012 0 ~0. 014 0[O], 0.005Al) produced by domestic 100 t EAF-LF-CC, 80 t, 100 t and 160 t BOF-LF-CC four process production line is carried out. Results show that the control characteristic of domestic 1215 low carbon high Sulphur free-cutting steel is to control Mn/S (3. 7 - 3. 9) of steel by suitable increasing Mn content in steel and for individual flow sheet is by decreasing S content in steel to get Mn/S =4. 4; the inclusion control of inclusion in steel produced by 160 t BOF flow sheet (Mn/S =3. 8, fluctuation of MnS inclusions area and length/width ratio are comparatively smaller) is better than that by others; due to smaller segregation of elements in casting billet and suitable controlling of cooling rate after rolling the steel produced by 80 t BOF flow sheet and 160 t flow sheet has no obvious banded structure, but by 100 t EAF flow sheet and 100 t BOF flow sheet the rating of banded structure is 3 ~4.