Structure Evolution of Grain-oriented 3.0% Si Steel with Low Temperature Slab Reheating in High Temperature Annealing

Fang Jianfeng1, Zhao Yu1, Tian Zhiling1, Li Jun2, Zhang Zhenzhen1   

  1. 1 State Key Laboratory of Advanced Steel Processes and Products, Central Iron and Steel Research Institute, Beijing 100081;
    2 Functional Materials Branch, Advanced Technology and Materials Co Ltd, Beijing 100081
  • Received:2010-03-01 Published:2010-08-01 Online:2022-11-21

摘要: 采用取向分布函数及金相分析方法研究了以Cu2S为主要抑制剂的低温板坯加热晶粒取向硅钢(%:0.04C、3.16Si、0.50Cu)在650~1 050℃高温退火中组织的演化过程。结果表明,该取向硅钢的初次再结晶温度为650~700℃,二次再结晶温度为1 000~1 050℃。初次再结晶后的主要织构强度以{111}〈110〉、 {112}〈110〉、 {111}〈112〉顺序减弱。初次再结晶组织的晶粒尺寸和织构强度在700~900℃变化很小,在900~1 000℃晶粒长大速度加快,{111}〈110〉、{112}〈110〉组分增强,而{111}〈112〉组分的强度基本保持不变。

关键词: 低温板坯加热, , 晶粒取向, Si钢, 退火, , 组织

Abstract:  The structure evolution of grain-oriented Si steel (%:0.04C,3. 16Si,0.50Cu) with    main    inhibitor    Cu2S and   low temperature   slab reheating   in   650~1050 ℃ high temperature annealing process has been   studied by orientation distribution   function   and metallographic   observation. Results   show  that  the  primary   and   secondary  recrystallization  temperature  of  the  grain-oriented  Si  steel  are  650~700  ℃  and   1000~1050  ℃  respectively;  the  intensity  of  main  texture  in  primary     recrystallized     steel     decreases     in     order     of{111}<110>,{112I<110>and{111}<112>,and     the     grain     size     and  intensity   of  texture   in   primary   recrystallized   structure   change   slightly   at   700~900℃,while   at   900~1000   ℃   the   velocity  of   grain    growth    accelerates    and    the{111}<110>    and{112}<110>    texture    components    intensify, but    the    intensity    of  {111}<112>  texture    component    is    almost    un-changed.