[1] 刘国勋、金属学原理.北京:冶金工业出版社,1983
[2] 杨觉先.金属塑性变形物理基础.北京:冶金工业出版社,1988
[3] Parks W H,Haggerty C S,Rock T R. Iron and Steel Engineer,1997, 76(10):35
[4] Langner H,Bleck W,Greisert C.Metallurgical Aspect of Ferites Hot Rolling.In Bleck W ed.Proceedings of Inter Symp on Modem L C and ULC Sheet Steel for Cold Forming. Ashen: Processing and Properties, 1998,301
[5] 马鸣图,沙维.材料科学和工程研究进展(第一集).北京:机械工业出版社,2000,590
[6] 马鸣图.我国汽车钢板研究与应用进展.钢铁,2001,36(8):64
[7] 王先进,茹铮,马衍伟.我国汽车用钢板的现状和研究进展钢铁,1998,33(10):1
[8] 马衍伟,王先进,孔冰玉.宝钢IF 钢生产工艺与改进建议.钢铁,1998,33(6):32
[9] 胡晓军.硫在Ti-IF钢中的作用.北京科技大学学报,2001,23(3):275
[10] Yoshinaga N.Precipitation Behavior of Sulfides in Ti-adled Utra Low-carbon Steels in Austenite. ISIJ Int,1994,34:24
[11] 余志祥.钢水精炼技术在武钢的开发应用.炼钢,2001,17(6):1
[12] 东涛,孟繁茂,傅俊岩.微合金化钢知识讲座.北京:北京理工大学出版社,2001,40
[13] 程国平,茹静,袁明生.钛铌添加量对超深冲IF钢板力学性能的影响.钢铁,1999,34(5):47
[14] Yoda Rika, Tsukatani lchiro, Inoue Tsuyoshi,et al.Effect of Chemical Composition on Recrystallization Behavior and r-value in Ti-added Ultra Low Carbon Sheet Steel. ISIJ International,1994,34(1):70
[15] Tither C,Garcia CI, Hua M,et al.Precipitation Behavior and Solute Effects in Interstitial Steels, Proceedings of International Forum for Physical Metallurgy of IF Steels.ISIJ International,1994(5):293
[16] 王作成,关小军,王先进,等.热轧工艺因素对拉延用热轧IF钢性能的影响.特殊钢,1999,20(2):43
[17] 陈新平,鲍平,蒋浩民.润滑条件对超深冲IF钢成形性能的影响.金属成形工艺,2002,20(2):8
[18] Meuleman D J,Siles J L,Zoidak J J. The Limiting Dome Height Test for Assessing the Formability of Sheet Steel.International Congress & Exposition, Detroit, Michigan, 1985
[19] 商建辉,王先进,蒋冬梅,等.卷取温度对T-IF钢第二相粒子及晶粒尺寸的影响.钢铁,2002,37(3):43
[20] Tither G,Carcia C I,Hua M,et al.Precipitation Behavior and Solute Effects in Interstitial-free Steels. Interational Forum for Physical Metallurgy of IF Steels, T.Sakuma, Tokyo: The lron and Steel Institute of Japan,1994,May 10-11,293
[21] Park,Kestens L,Jonas J J.Effect of Internal Stresses in Cold Rolled IF Steel on the Orientations of Recrystallized Grains.ISIJ Interational,2000,40(4):393
[22] 李艳娇,刘战英,李晋霞,等.冷轧压下率对铁素体区热轧Ti-IF钢冷轧板深冲性能的影响.钢铁研究学报,2003,15(1):34
[23] 刘战英,李晋霞,刘相华,等.两次冷轧压下率分配对IF钢深冲性能的影响.东北大学学报(自然科学版),2004,25(3):254
[24] 马虹蔚.无间隙原子IF钢罩式退火工艺的研究.轧钢,2002,19(1):18
[25] 茹铮,曹全禹,彭璇,等.IF钢冷轧薄板罩式退火工艺的优化.北京科技大学学报,2000,22(3):223
[26] 叶卫平 .IF钢SEM原位加热再结晶过程的研究.特殊钢, 2001,22(4):13
[27] 叶卫平.IF钢罩式退火再结晶晶粒分布函数.特殊钢,2001,22(2):22
[28] Jonas J J,Urabe T.Oriented Nucleation and Selective Growth during on Annealing df IF Steels. International Forum for Physical Metallurgy of IF Steels.Tokyo,1994
[29] Bamett M R,Kestens L. Formation of {111}and {111}Textures in Cold Rolled and Annealed IF Sheet Steel.ISIJ International,1999,39(9):923
[30] 李伯龙,张宁,刘庆.用电子背散射衍射技术研究IF-钢再结晶行为.电子显微学报,2002,21(5):727
[31] 赵昆,李自刚,何晓明,等.Ti-IF钢铁素体区热变形行为研究和Zener-Hollomen参数方程的建立.材料科学与工艺,2000,8(4):6
[32] 初元璋,潘岩 .IF钢的二次加工脆性及其评定方法.特殊钢,2000,21(1):36
|