[1] 董 瀚,先进汽车钢扁平材和长形材的研发进展[C].2009年汽车用钢生产及应用技术国际研讨会,大连,2009.
[2] Sato M Utsumi Y, Watanabe K. Ultra-High-Strength, Quench-Type, Hot-Rolled Steel Sheets of 1620MPa Grade for Automobile Door Impact Beams [J]. Kobeleo Technology Review ,2008,28: 13-17.
[3] Zmik J,Mamuzic I, Dobatkin SV. Recent Progress in High Strength Low Carbon Steels [C]. Metabk,2006,45(4):323-331.
[4] Hayashi H, Nakagawa T. Recent Trends in Sheet Metals and Their Formability in Manufacturing Automotive Panels[J]. Journal of Materials Processing Technology, 1994,46(3-4):455-487.
[5] Kwon O J,Lee K Y,Kim G S,et al. New Trends in Advanced High Strength Steel Developments for Automotive Application[J]. Materials Science Forum ,2010,638-642:136-141.
[6] Sugimoto K,Iida T,Sakaguchi J,et al. Retained Austenite Characteristics and Tensile Properties in a TRIP Type Bainitic Sheet Steel [J]. ISIJ Internal, 2000,40(9) ;902-908.
[7] 董 翰.第三代汽车钢原理及其温成形技术[C].2O15中国汽车轻量化技术国际研讨会,重庆,2015.
[8] Sugimoto K,Yu B ,Mukai Y,Ikeda S. Microstructure and Formability of Aluminum Bearing TRIP-Aided Steels with Annealed Martensite Matrix [J]. ISIJ,International,2005,45 (8) : 1194-1200.
[9] Frommeryer G,Brtix U,Neumann P. Supra-Ductile and High-Strength Manganese-TRIP/TWIP Steels for High Energy Absorption Purposes. ISIJ International,2003,43(3) :438^46.
[10] Meng C F,Zhang L,Wang C Y,et ai. Microstructure and Mechanical Properties of 20Si2CrNi3MoV Steel Treated by HDQP Process [J]. Journal of Iron and Steel Research, International, 2017,24; 1137-1142.
[11] Park K T. Tensile Deformation of Low-Density Fe-Mn-Al-C Austenitic Steels at Ambient Temperature [J]. Scripta Materialia,2013, 68 :375-379.
[12] Wang C Y,Chang Y,Yang J ,Cao W Y,et al. Work Hardening Behavior and Stability of Retained Austenite for Quenched and Partitioned Steels [J]. Journal of Iron and Steel Research, International, 2016,23:130437.
[13] Li Z C, Ding H, Misra R D K, Cai Z H. Deformation Behavior in Cold Rolled Medium-Manganese TRIP Steel and Effect of Pre-Strain on the Luders bands [J]. Materials Science and Engineering A, 2017,679-230-239.
[14] Li W S,Gao H Y,Nakashima H, et al. In-Situ Study of The Deformation-Induced Rotation and Transformation of Retained Austenite in a Low-Carbon Steel Treated by Be Quenching and Partitioning Process. [J]. Materials Science and Engineering A, (2016):649 417-425.
[15] Song C H,Yu H,Li L L, et al. The Stability of Retained Austenite at Different Locations During Straining of I & Q & P Steel [J]. Materials Science and Engineering: A ,2016,670:326-334.
[16] Hu H J,Zhao A M,Yin Z K,et al. Effect of Pre-Strain on Mechanical Properties and Hardening Behavior of TRIP Steel [J]. Transaction of Materials and Heat Treatment ,2016,37(5) :128-132.
|