SiCaBa合金对55SiCr弹簧钢的脱氧脱硫及夹杂物控制研究
刘锦文, 铁占鹏, 郭路召, 张硕, 张家泉, 唐海燕
Study on Deoxidation, Desulfurization and Inclusion Control of SiCaBa Alloy on Spring Steel 55SiCr
Liu Jinwen, Tie Zhanpeng, Guo Luzhao, Zhang Shuo, Zhang Jiaquan , Tang Haiyan
特殊钢
.
2020, (3): 20
-24
.