邢钢400系低碳易切削不锈钢控碳工艺实践
白李国, 王欣, 李广斌, 冯兴磊, 吴广海, 杨强强
Process Practice on Carbon Control of Low Carbon 400 Series Free Cutting Stainless Steel at Xingtai Steel
Bai Liguo ' , Wang Xin, , Li Guangbin, , Feng Xinglei, Wu Guanghai , Yang Qiangqiang
特殊钢
.
2020, (4): 22
-25
.