80 t BOF-LF-RH流程GCrl5钢超深脱硫的生产实践
赵世杰, 轩振博, 冯文甫, 刘学强, 范建英, 霍立国
Production Practice of Ultra Deep Desulphurization of Steel GCrl5 by 80 t BOF-LF-RH Process
Zhao Shijie , Xuan Zhenbo , Feng Wenfu, Liu Xueqiang , Fan Jianying , Huo Liguo
特殊钢
.
2020, (5): 42
-44
.