AISI 410SS钢Φ200 mm锻材轴心晶间裂原因分析与工艺改进
张军, 李造宇, 杨玲, 郑振宇, 杨娥, 伍伟
Cause Analysis and Process Improvement of Centre Intergranular Crack of Φ200 mm Forging of Steel AISI 410SS
Zhang Jun, , Li Zaoyu , Yang Ling , Zheng Zhenyu, , Yang E , Wu We
特殊钢
.
2020, (5): 52
-54
.