160 mm x 160 mm连铸坯结晶器电磁搅拌对钢液流场影响的数值模拟
党爱国, 钟保军, 田新中, 李永超
Numerical Simulation on Effect of Electromagnetic Stirring in 160 mm x 160 mm Billet Mould on Flow Field of Molten Steel
Dang Aiguo, Zhong Baojun, Tian Xinzhong , Li Yongchao
特殊钢
.
2020, (6): 6
-11
.