连铸板坯快冷试验分析Q345D包晶钢板坯角部横裂成因和工艺改进
颜慧成, 成旭东, 巩彦坤, 张凯, 马静超
Analysis on Formation of Transverse Corner Cracks of Slab of Peritectic Steel Q345D by Slab Quenching Test and Process Improvement
Yan Huicheng, Cheng Xudong, Gong Yankun, Zhang Kai , Ma Jingchao
特殊钢
.
2019, (5): 64
-66
.