胀断连杆用C70S6 BY钢连轧材探伤不合格原因分析和工艺改进
康港'刘向艳'杨建华翟军'孙琦'穆立峰'马群
Analysis on Cause of Off-Qualified Continuous-Rolling Products of Steel C70S6 BY by Ultrasonic Detection and Process Improvement
Kang Tian' , Liu Xiangyan , Yang Jianhua, Zhai Jun , Sun Qi , Mu Lifeng and Ma Qun
特殊钢
.
2019, (2): 21
-23
.