自耗电极冶金质量对G20CrNi2Mo轴承钢电渣锭洁净度的影响
李世健, 成国光, 苗志奇, 陈列, 姜新岩
Effect of Consumable Electrode Metallurgical Quality on Cleanliness of Bearing Steel G20CrNi2Mo ESR Ingot
Li Shijian , Cheng Guoguang, Miao Zhiqi, Chen Lie , Jiang Xinyan
特殊钢
.
2018, (6): 6
-10
.