120 t RH自然脱碳精炼低碳钢QD08的生产实践
李海, 刘列喜, 张洪彪, 介瑞华, 王立青, 陆曼, 徐雷
Production Practice for Low Carbon Steel QD08 Steelmaking by Natural Decarburization during 120 t RH Refining Process
Li Hai, Liu Liexi, Zhang Hongbiao, Jie Ruihua, Wang Liqing, Lu Man , Xu Lei
特殊钢
.
2018, (3): 13
-16
.