固溶温度对奥氏体不锈钢022Cr24Ni17Mo5Mn6NbN组织和性能的影响
史咏鑫, 李青, 钟庆元, 冯文静, 常松, 王敏
Effect of Solution Temperature on Microstructure and Properties of Super Austenitic Stainless Steel 022Cr24Ni17Mo5Mn6NbN
Shi Yongxin, Li Qing, Zhong Qingyuan, Feng Wenjing, Chang Song , Wang Min
特殊钢
.
2022, (2): 82
-84
.