高强度汽车紧固件用钢SCr440连续冷却和等温冷却组织转变研究及应用
李战卫, 于学森, 沈奎, 张宇, 刘卫
Study on Continuous Cooling and Isothermal Cooling Microstructure Transformation of High Strength Steel SCr440 for Automotive Fasteners and Application
Li Zhanwei, Yu Xuesen, Shen Kui, Zhang Yu, Liu Wei
特殊钢
.
2022, (2): 90
-94
.