YG1900超高强度钢性能指标离散机理分析及工艺改进
董晓亮, 张秀丽, 许广鹏, 郑振宇, 曹广, 廖凯
Mechanism Analysis and Process Improvement of YG1900 Ultra-High-Strength Steel's Non-Uniform Properties
DONG Xiaoliang , ZHANG Xiuli, XU Guangpeng , ZHENG Zhenyu, CAO Guang, LIAO Kai
特殊钢
.
2022, (3): 52
-55
.