膨胀及原位观测法研究低碳贝氏体钢轨U25CrNi连续冷却相变
万菲, 刘晓卫, 朱敏, 闻臻
Investigation on Continuous Cooling Transformation Process of Low Carbon Bainite Rail Steel U25CrNi by Dilatation and in-situ Observation Method
WAN Fei, LIU Xiaowei , ZHU Min, WEN Zhen
特殊钢
.
2022, (3): 79
-84
.