220mm x 1600mm板坯连铸浸入式水口倾角优化的数值模拟和应用
宁林新, 解家英, 刘金刚, 张利君
Numerical Simulation on Optimization of Inclination of Submerged Nozzle for 220mm x 1600mm Slab Casting and Application
Ning Linxin , Xie Jiaying , Liu Jingang , Zhang Lijun
特殊钢
.
2018, (1): 9
-12
.