低钛高炉渣应用于HRB400E螺纹钢100t LF精炼的工业试验
王宝华, 宫永煜, 张明博, 黄世平, 宁树博
Commercial Pilot Production of Threading Steel HRB400E 100t LF Refining by Using Low Titanium Blast Furnace Slag
Wang Baohua , Gong Yongyu , Zhang Mingbo , Huang Shiping , Ning Shubo
特殊钢
.
2018, (1): 28
-33
.