唐钢60t转炉石灰石替代部分石灰造渣炼钢的工业试验
李晨晓, 郝华强, 王书桓, 赵定国, 陈建军, 刘善喜
Commercial Pilot Production on Replacing Partial Lime in Slag by Limestone in 60t Converter Steelmaking at Tangsteel
Li Chenxiao, Hao Huaqiang, Wang Shuhuan, Zhao Dingguo, Chen jianjun, Liu Shanxi
特殊钢
.
2017, (6): 16
-18
.