800℃至500℃冷却时间对9Ni低温钢相转变行为和微观结构的影响
杨秀芝, 华文林, 杨春杰, 董春法
Effect of Cooling Time from 800℃ to 500℃ on Phase Transition Behavior and Microstructure of Low Temperature Steel 9Ni
Yang Xiuzhi , Hua Wenlin , Yang Chunjie , Dong Chunfa
特殊钢
.
2017, (5): 10
-12
.