卷取后冷却工艺对700 MPa微合金钢带材组织和性能的影响
董方, 武利平, 宿成, 闫瑞军, 沈国慧, 刘月
Effect of Cooling Process after Coiling on Structure and Properties of 700 MPa Microalloying Steel Strip
Dong Fang , Wu Liping , Su Cheng , Yan Ruijun , Shen Guohui , Liu Yue
特殊钢
.
2017, (5): 61
-64
.