冷作模具钢Crl2MoV 40 t EAF-LF.VD-模铸冶炼工艺优化实践
梁新腾, 谢珍勇, 孙彦辉, 王建, 蔡武
Process Optimization Practice of 40 t EAF-LF-VD-Mould Casting Steelmaking for Cold-Working Die Steel Crl2MoV
Liang Xinteng', Xie Zhenyong, Sun Yanhui, Wang Jian , Cai Wu
特殊钢
.
2017, (4): 32
-34
.