60t AOD-LF-CCM 流程冶炼清洁球用超低[C+N]不锈钢0Cr13的工艺实践
叶凡新, 冯文甫, 郭志彬, 王晓亮, 曹红波, 吴广海
Process Practice of Steelmaking of Ultra Low [C+N] Stainless Steel 0Cr13 for Cleaning Ball by 60t AOD-LF-CCM Flowsheet
Ye Fanxin , Feng Wenfu , Guo Zhibin , Wang Xiaoliang , Cao Hongbo , Wu Guanghai
特殊钢
.
2017, (2): 23
-25
.