NM450D 耐磨钢-Q235B 碳钢复合板的轧制和热处理工艺对组织、性能的影响
邱俊, 程晓茹, 兰昆, 雷冬, 王煜, 黄大军
Effect of Rolling and Heat-Treatment on Structure and Properties of Wear-Resistant Steel NM450D-Carbon Steel Q235B Clad Plate
Qiu Jun , Cheng Xiaoru , Lan Kun , Lei Dong , Wang Yu , Huang Dajun
特殊钢
.
2017, (2): 56
-59
.