100 t转炉“留渣+双渣”提钒,半钢冶炼低磷钢渣成分控制的工艺实践
韩宇, 张明博, 冷何晴, 王鹏, 张东
Practice on Control of Slag Ingredient for Extracted-Vanadium Semi-Steel 100 t BOF Steelmaking Low Phosphorus Steel by “ Slag-Remaining + Double Slag” Process
Han Yu , Zhang Mingbo, He Qing , Wang Peng , Zhang Dong
特殊钢
.
2017, (1): 27
-30
.