60 t AOD全铁水精炼400系不锈钢热补偿技术的工艺实践
叶凡新, 冯文甫, 郭志彬, 王晓亮, 曹红波, 吴广海
Process Practice of Thermal Compensation Technology for Refining 400 Series Stainless Steels in a 60 t AOD with Hot Metal
Ye Fanxin, Feng Wenfu, Guo Zhibin, Wang Xiaoliang, Cao Hongbo , Wu Guanghai
特殊钢
.
2016, (6): 44
-46
.