超低碳钢150 t转炉冶炼过程超低硫的控制和工艺实践
张振申, 程官江, 王新志, 王中岐, 夏志升
Control of Ultra-Low Sulphur during 150 t BOF Ultra-Low Carbon Steel Steelmaking and Process Practice
Zhang Zhenshen, Cheng Guanjiang, Wang Xinzhi, Wang Zhongqi , Xia Zhisheng
特殊钢
.
2016, (6): 47
-51
.