电渣重熔对高氮17Cr-17Mn-2Mo奥氏体不锈钢冶金质量和性能的影响
姚春发, 邢长军, 孙国强, 吴 林, 宁小智, 胡秋利
Effect of Electro-Slag Remelting on Metallurgical Quality and Properties of High Nitrogen 17Cr-17Mn-2Mo Austenite Stainless Steel
Yao Chunfa, Xing Changjun, Sun Guoqiang, Wu Lin, Ning Xiaozhi , Hu Qiuli
特殊钢
.
2017, (1): 46
-48
.