固溶温度对00Cr13Ni7Co5Mo4W马氏体时效不锈钢组织和耐点腐蚀的影响
姜越, 黎士强, 张月, 祖红梅
Effect of Solid-Solution-Treated Temperature on Structure and Pitting Corrosion Resistance of Maraging Stainless Steel 00Cr13Ni7Co5Mo4W
Jiang Yue, Li Shiqiang, Zhang Yue , Zu Hongmei
特殊钢
.
2015, (6): 42
-44
.