热轧线材中心偏析对油淬回火55SiCrA弹簧钢力学性能的影响
孟耀青, 郑永瑞, 李拥军, 赵昊乾, 王伟
Effect of Center Segregation of Hot-Rolled Rod on Mechanical Properties of Oil-Quenched and Tempered Spring Steel 55SiCrA
Meng Yaoqing , Zheng Yongrui , Li Yongjun , Zhao Haoqian , Wang Wei
特殊钢
.
2015, (5): 64
-66
.