熔盐电沉积过程温度对1.6Si无取向硅钢Si扩散的影响
李慧, 梁精龙, 赵晓萍, 李运刚, 张芬萍
Effect of Temperature on Diffusion of Si in 1.6Si Non-Oriented Silicon Steel during Molten Salt Electro-Deposit Process
Li Hui, Liang Jinglong, Zhao Xiaoping, Li Yungang, Zhang Fenping
特殊钢
.
2014, (6): 12
-14
.