避免原辅料对KB-150 t BOF-RH-CC流程MA超低碳钢水增碳的生产实践
邓力, 彭其春, 宋佳霖, 邱雷, 盛喜松, 邓品团
Production Practice of Avoiding Raw and Supplement Materials on Increase Carbon in MA Ultra-Low Carbon Steel Liquid during KB-150 t BOF-RH-CC Flowsheet
Deng Li , Peng Qichun , Song Jialin , Qiu Lei , Sheng Xisong , Deng Pintuan
特殊钢
.
2015, (2): 32
-35
.