异型坯连铸长水口浸入深度对36 t中间包流场和温度场的影响
阮飞, 赵凤光, 富晓阳, 刘卓承, 杨吉春, 张捷宇
Influence of Immersion Depth of Long Nozzle on Flow Field and Temperature Field of Liquid Steel in a 36 t Tundish during Profiled Bloom Casting
Ruan Fei , Zhao Fengguang, Fu Xiaoyang, Liu Zhuocheng, Yang Jichun, Zhang Jieyu
特殊钢
.
2015, (1): 9
-13
.