终轧温度和晶粒度对非调质钢JGF45V冲击功的影响
韩怀宾, 宋建锋, 王清波, 白瑞娟, 王维, 虞学庆,
Effect of Finishing Rolling Temperature and Grain Size on Impact Energy of Non-Quenched-Tempered JGF45V Steel
Han Huaibin, Song Jianfeng , Wang Qingbo, Bai Ruijuan , Wang Wei , Yu Xueqing
特殊钢
.
2021, (3): 67
-70
.