50 t EAF-AOD-LF-VD-CC-轧制高碳不锈钢9Cr18盘条的工艺实践
李忠之, 杨庆敏, 俞亚杰, 于全功, 聂显飞, 周一玲
Process Practice of Rod Coil of High Carbon Stainless Steel 9Cr18 Produced by 50 t EAF-AOD-LF-VD-CC-Rolling Flow Sheet
Li Zhongzhi , Yang Qingmin , Yu Yajie , Yu Quangong , Nie Xianfei , Zhou Yiling
特殊钢
.
2014, (5): 37
-39
.