优化连铸工艺和化学成分改善耐蚀钢G7624表面质量的生产实践
王利伟, 贾育华, 王笑丹, 邸永田, 张治广, 田新中
Production Practice of Improving Surface Quality of Corrosion Resistant Steel G7624 by Optimizing Concasting Parameters and Chemical Composition
Wang Liwei , Jia Yuhua , Wang Xiaodan , Di Yongtian , Zhang Zhiguang , Tian Xinzhong
特殊钢
.
2014, (5): 40
-42
.