结晶器保护渣对300mm×360mm低碳钢连铸坯表面质量的影响和成分优化
曾亚南, 孙彦辉, 艾西, 马志飞, 刘瑞宁, 刘泳
Effect of Mold Powder on Surface Quality of 300 mm x 360 mm Casting Bloom of Low Carbon Steel and Ingredient Optimization
Zeng Yanan, Sun Yanhui , Ai Xi, Ma Zhifei, Liu Reining , Liu Yong
特殊钢
.
2014, (4): 24
-27
.