25SiMn2钢部分170 mm连铸板坯吊运断裂原因分析和改进措施
苏春霞, 陈本文, 付超, 孙殿东, 王 勇
An Analysis on Crane- Conveying Fracture of Partial 170 mm Casting Slab of Steel 25SiMn2 and Improving Measures
Su Chunxia, Chen Benwen, Fu Chao, Sun Diandong , Wang Yong
特殊钢
.
2014, (4): 34
-35
.