GCr15轴承钢ø380 mm连铸圆坯V-偏析的宏观与微观形貌分析
黄拓, 任金朝, 马忠伟, 王明林, 张慧
An Analysis on Morphology of Macro and Microstructure of V-Segregation in ø380 mm Continuous Casting Bloom of Bearing Steel GCr15
Huang Tuo, Ren Jinzhao, Ma Zhongwei, Wang Minglin, Zhang Hui
特殊钢
.
2014, (4): 48
-51
.