高牌号无取向硅钢CSP流程铸坯及热轧板的组织和夹杂物分析
马良, 荣哲, 项利, 仇圣桃, 赵沛
An Analysis on Structure and Inclusions in CSP Casting Slab and Hot Rolled Plate of High Grade Non-Oriented Silicon steel
Ma Liang, Rong Zhe, Xiang Li, Qiu Shengtao , Zhao Pei
特殊钢
.
2013, (4): 59
-61
.