150 t BOF-LF-VD-CC流程无铝脱氧工艺高速轨钢冶炼过程的夹杂物行为
刘平, 李笑英, 智建国, 陈爱梅
Behavior of Inclusions in 150 t BOF-LF-VD-CC Flow Sheet Non-Aluminium Deoxidation Steelmaking Process of High-Speed Rail Steel
Liu Ping , Li Xiaoying , Zhi Jianguo , Chen Aimei
特殊钢
.
2013, (5): 51
-53
.