210 t顶底复吹转炉-RH流程IF钢板坯连铸钢水温降规律的研究
王毓男, 包燕平, 崔衡, 陈斌, 季晨曦
Study on Regularity of Temperature Reduction of IF Steel Slab Casting Liquid with 210 t Top and Bottom Combined Blown Converter-RH Flow Sheet
Wang Yunan, Bao Yanping, Cui Heng, Chen Bin, Ji Chenxi
特殊钢
.
2011, (1): 40
-43
.