固溶处理对超低碳奥氏体不锈钢00Cr24Ni13铸坯δ-铁素体转变的影响
舒玮, 廉晓洁, 张寿禄, 李建春, 罗刚
Effect of Solid Solution Treatment on δ-Ferrite Transformation in Casting Slab of Ultra-Low Carbon Austenite Stainless Steel 00Cr24Ni13
Shu Wei, Lian Xiaojie, Zhang Shoulu, Li Jianchun, Luo Gang
特殊钢
.
2013, (2): 62
-64
.