时效处理对15-5PH沉淀硬化马氏体不锈钢组织和力学性能的影响
裴海祥, 王西涛, 王立新, 邢丽娜
Effect of Ageing Treatment on Structure and Mechanical Properties of Precipitation-Hardening Martensite Stainless Steel 15-5PH
Pei Haixiang, Wang Xitao , Wang Lixin, Xing Lina
特殊钢
.
2012, (5): 47
-48
.